Synthesis of yttrium aluminum garnet ceramic powder doped with ruthenium
In the course of the work, samples of ceramic powders of yttrium-aluminum garnet doped with ruthenium ions were obtained. The introduced amount of ruthenium was 5 and 10 wt.%, respectively. The annealing temperatures were 1150 and 1600°C. In the course of the work, changes in the morphology of ceram...